MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 7001-T75
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Key Words: UNS A97001; Aluminium 7001-T75; AA7001-T75; Al7001-T75
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.84 g/cc0.103 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 155155500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 198198Converted from Brinell Hardness Value
Hardness, Rockwell A 54.454.4Converted from Brinell Hardness Value
Hardness, Rockwell B 8989Converted from Brinell Hardness Value
Hardness, Vickers 181181Converted from Brinell Hardness Value
Tensile Strength, Ultimate 580 MPa84100 psi
Tensile Strength, Yield 495 MPa71800 psi
Elongation at Break 12 %12 %In 5 cm; Sample 1.6 mm thick
Modulus of Elasticity 71.0 GPa10300 ksiAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus. Estimated from trends in similar Al alloys.
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Shear Modulus 27.0 GPa3920 ksiEstimated from similar Al alloys.
Shear Strength 340 MPa49300 psiEstimated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000500 ohm-cm0.00000500 ohm-cmEstimated from other heat treatments.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
 25.0 µm/m-°C
@Temperature 20.0 - 300 °C
13.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.860 J/g-°C0.206 BTU/lb-°FEstimated from trends in similar Al alloys.
Thermal Conductivity 140 W/m-K972 BTU-in/hr-ft²-°FEstimated from other heat treatments.
Melting Point 477 - 627 °C891 - 1160 °F
Solidus 477 °C891 °F
Liquidus 627 °C1160 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 87 %87 %As remainder
Chromium, Cr 0.18 - 0.35 %0.18 - 0.35 %
Copper, Cu 1.6 - 2.6 %1.6 - 2.6 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 2.6 - 3.4 %2.6 - 3.4 %
Manganese, Mn <= 0.20 %<= 0.20 %
Silicon, Si <= 0.35 %<= 0.35 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn 6.8 - 8.0 %6.8 - 8.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7001-T6; 7001-T651
Aluminum 7005-T53
Aluminum 7034-T6
Aluminum 7005-T6, 7005-T63, and 7005-T6351
Aluminum 7005-O

MA7001T75 / 9522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.