MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AK Steel Hot Rolled Carbon Steel, Drawing Steel (DS Type B), Standard Grade
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: DS is made by adding aluminum to the molten steel and may be used in drawing applications.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 5656
Tensile Strength, Ultimate 330 MPa47900 psi
Tensile Strength, Yield 240 MPa34800 psi
Elongation at Break 41 %41 %
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000142 ohm-cm0.0000142 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.481 J/g-°C
@Temperature 50.0 - 100 °C
0.115 BTU/lb-°F
@Temperature 122 - 212 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel Cold Rolled Carbon Steel, Drawing Steel (DS Type B), Standard Grade
ASTM A131 Steel, Grade DS
AK Steel Hot Rolled Carbon Steel, Commercial Steel (CS Type B), Standard Grade
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
AISI 1015 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round

NAKS001 / 14604

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.