MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® BKV 15 H2.0 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: CoPA, injection molding grade, 15% glass fibers, good heat-ageing resistance

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.6 %2.6 %50% RH; ISO 62
Water Absorption at Saturation 8.5 %8.5 %IOS 62
Linear Mold Shrinkage, Flow 0.0029 cm/cm0.0029 in/in150x105x3; ISO 2577
Linear Mold Shrinkage, Transverse 0.0088 cm/cm0.0088 in/in150x105x3; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 170 MPa24700 psiISO 2093-1
Tensile Strength at Break 125 MPa18100 psi5 mm/min; ISO 527-1,-2
Elongation at Break 2.5 %2.5 %5 mm/min; ISO 527-1,-2
Tensile Modulus 5.30 GPa769 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 180 MPa26100 psi2 mm/min; ISO 178-A
Flexural Yield Strength 170 MPa
@Strain 3.5 %
24700 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 4.70 GPa682 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 4.0 %4.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -40.0 °C
<= 4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  55.0 kJ/m²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 <= 1.00 J/cm²
@Temperature -40.0 °C
<= 4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 180-1A
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 375 V375 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 213 °C415 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75-1,-2
Deflection Temperature at 8.0 MPa 60.0 °C140 °FISO 75-1,-2
Vicat Softening Point  >= 200 °C
@Load 5.10 kg
>= 392 °F
@Load 11.2 lb
120°C/h; ISO 306
 200 °C
@Load 5.10 kg
392 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
Oxygen Index 22 %22 %Method A; ISO 4589-2
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695-2-12
Shrinkage, MD 0.080 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.080 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction 150x105x3; ISO 2577
Shrinkage, TD 0.21 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.21 %
@Treatment Temp. 248 °F,
Time 4.00 hour
150x105x3; ISO 2577
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °F
Mold Temperature 80.0 °C176 °F
Back Pressure 60.0 MPa8700 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 15 H2.0 901510 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3EG3 BK00564 15% Glass Filled PA6 (Dry)
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned)
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry)

PLANW9518 / 208159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.