MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent choice for decorative structural applications.

Applications include automobile molding and trim, wheel cover, conveyor belts, kitchen equipment, roof draining systems, hose clamps, springs, truck and trailer bodies, railway and subway cars. By varying the chemical composition within the limits set by the ASTM Specifications and by temper rolling, a broad range of magnetic and mechanical properties can be obtained for a variety of applications.

Information provided by Allegheny Ludlum Corporation.

Key Words: ASTM A240; ASTM A666
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.03 g/cc0.290 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 297297
Hardness, Rockwell C 3232
Tensile Strength, Ultimate >= 1034 MPa>= 150000 psi
Tensile Strength, Yield >= 758 MPa
@Strain 0.2 %
>= 110000 psi
@Strain 0.2 %
Elongation at Break >= 18 %>= 18 %in 2" (50 mm)
Modulus of Elasticity 185 GPa26800 ksias rolled longitudinal
 186 GPa27000 ksias rolled transverse
Compressive Yield Strength 621 MPa90100 psilongitudinal
 979 MPa142000 psitransverse
Fatigue Strength 379 MPa55000 psiendurance limit; test details not reported
Charpy Impact 150 J111 ft-lb
 150 J
@Temperature -73.0 °C
111 ft-lb
@Temperature -99.4 °F
 150 J
@Temperature 196 °C
111 ft-lb
@Temperature 385 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000720 ohm-cm0.0000720 ohm-cm
Magnetic Permeability <= 1.02<= 1.02typically < 1.02 at 200H; increases with cold work.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.6 µm/m-°C
@Temperature 20.0 - 100 °C
9.22 µin/in-°F
@Temperature 68.0 - 212 °F
 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.78 µin/in-°F
@Temperature 68.0 - 572 °F
 18.6 µm/m-°C
@Temperature 20.0 - 500 °C
10.3 µin/in-°F
@Temperature 68.0 - 932 °F
 19.5 µm/m-°C
@Temperature 20.0 - 700 °C
10.8 µin/in-°F
@Temperature 68.0 - 1290 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.3 W/m-K
@Temperature 100 °C
113 BTU-in/hr-ft²-°F
@Temperature 212 °F
 21.4 W/m-K
@Temperature 500 °C
149 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1399 - 1421 °C2550 - 2590 °F
Solidus 1399 °C2550 °F
Liquidus 1421 °C2590 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe 70.7 - 78.0 %70.7 - 78.0 %as balance
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 6.0 - 8.0 %6.0 - 8.0 %
Nitrogen, N <= 0.10 %<= 0.10 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eagle Brass 301 Austenitic Stainless Steel, 1/2 Hardened
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100)
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100)
AK Steel 301 Austenitic Stainless steel
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100)

NL3012 / 17837

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.