MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Equate EMDA-6200 HDPE Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for high-speed production of high quality bottles. The bottles have excellent environmental stress cracking resistance and a good balance of rigidity and impact strength. They are easily trimmed and exhibit excellent surface attributes.

Applications: EMDA-6200 is intended for producing containers of up to 10 liter capacity for packaging household and industrial chemicals (detergents, bleach, fabric softeners, etc.) toiletries, cosmetics and food products. It is also suitable for producing thin-walled parts and household items. In addition EMDA-6200 can also be used successfully for extruding sheets and profiles including corrugated drainage pipes

Information provided by Equate

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D792
Environmental Stress Crack Resistance 50 hour50 hourF50; ASTM D1693 B
Melt Flow 0.40 g/10 min
@Load 2.16 kg
0.40 g/10 min
@Load 4.76 lb
ASTM D1238
High Load Melt Index 29 g/10 min
@Load 21.6 kg
29 g/10 min
@Load 47.6 lb
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Break 1140 %1140 %ASTM D638
Flexural Modulus 1.25 GPa181 ksiASTM D790
Crush Resistance 50.0 kg110 lb (mass)41g Boston Round Quart Bottle; ASTM D2659
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C66.7 µin/in-°FASTM D969
Melting Point 135 °C275 °FEquate Test Method
Crystallization Temperature 112 °C234 °FEquate Test Method
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648
Vicat Softening Point 125 °C257 °FASTM D1525
Brittleness Temperature <= -100 °C<= -148 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Zone 1 175 - 180 °C347 - 356 °F
Zone 2 185 - 190 °C365 - 374 °F
Zone 3 185 - 190 °C365 - 374 °F
Zone 4 185 - 190 °C365 - 374 °F
Adapter Temperature 185 - 190 °C365 - 374 °F
Die Temperature 185 - 190 °C365 - 374 °F
Melt Temperature 200 - 215 °C392 - 419 °FIntermittent Machines
 215 °C419 °F90 RPM
 220 °C428 °F130 RPM
Head Temperature 185 - 190 °C365 - 374 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Equate EGDA-6888 HDPE Film Extrusion Resin
Equate EMDA-6147 HDPE Blow Molding Resin
Equate EFDA-7047 LLDPE Film Extrusion Resin
Equate EFDC-7050 LLDPE Film Extrusion Resin
Equate EFDC-7087 LLDPE Film Extrusion Resin

PEQUAT902 / 150430

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.