MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® T 84 Polycarbonate/ABS Blend  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Easier flowing than BAYBLEND T 85 MN.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC + ABS; Poly(Acrylonitrile-Butadiene-Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Moisture Absorption at Equilibrium 0.20 %0.20 %50% RH
Water Absorption at Saturation 0.70 %0.70 %
 0.70 %0.70 %
Melt Flow 19 g/10 min
@Load 5.00 kg,
Temperature 260 °C
19 g/10 min
@Load 11.0 lb,
Temperature 500 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psi
Elongation at Break >= 50 %>= 50 %Nominal
Elongation at Yield 4.0 %4.0 %
Tensile Modulus 2.20 GPa319 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  2.0
@Frequency 100 Hz
2.0
@Frequency 100 Hz
 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
Dielectric Strength 24.0 kV/mm610 kV/in
Dissipation Factor  0.0040
@Frequency 100 Hz
0.0040
@Frequency 100 Hz
 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
120 - 180 sec
@Thickness 0.118 in
UL Rating PLC 5 (120-180 sec)
Comparative Tracking Index 250 V250 V
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 3.00 mm
15 - 30 sec
@Thickness 0.118 in
UL Rating PLC 3 (15-30 sec)
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
UL Rating PLC 0 (>120 arcs)
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 85.0 µm/m-°C
@Temperature 20.0 °C
47.2 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 128 °C262 °F
Deflection Temperature at 1.8 MPa (264 psi) 108 °C226 °F
Vicat Softening Point 127 °C261 °F
UL RTI, Electrical 60.0 °C
@Thickness 1.50 mm
140 °F
@Thickness 0.0591 in
UL RTI, Mechanical with Impact 60.0 °C
@Thickness 1.50 mm
140 °F
@Thickness 0.0591 in
UL RTI, Mechanical without Impact 60.0 °C
@Thickness 1.50 mm
140 °F
@Thickness 0.0591 in
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Oxygen Index 24 %24 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Molded
Covestro Bayblend® T 44 Polycarbonate/ABS Blend
Covestro Bayblend® T65 AT PC/ABS Blend
Overview of materials for Polypropylene, Flame Retardant
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy

PBA050 / 26677

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.