MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Elements Tin Nanoparticles
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: General Description

Tin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specific surface area (SSA) in the 30 – 60 m 2 /g range and also available in with an average particle size of 80 nm range with a specific surface area of approximately 12 m 2 /g. Nano Tin Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Tin nanocrystals include in transparent ant-static film, as an anti-microbial, anti-biotic and anti-fungal agent when doped with silver and incorporated in coatings, plastics, nanofiber, bandages and textiles. Further research is being done for their potential as confined acoustic and optic phonons and for their electrical, biomedical and bioscience properties. Tin Nano Particles are generally immediately available in most volumes.

Key Words: Formula: Sn; CAS Number: 7440-31-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.31 g/cc0.264 lb/in³
Particle Size 0.010 - 0.020 µm0.010 - 0.020 µm
 0.080 µm0.080 µm
Specific Surface Area 12 m²/g12 m²/g
 30 - 60 m²/g30 - 60 m²/g
Molecular Weight 118.69 g/mol118.69 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 231.93 °C449.47 °F
Boiling Point 2602 °C4716 °F
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tin, Sn (Gray)
Tin (II) Acetate, Sn(C2H3O2)2
Tin (II) Hydroxide, Sn(OH)2
Tin (II) Pyrophosphate, Sn2P2O7
Tin (IV) Chromate, Sn(CrO4)2

EJAMER85 / 5568

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.