MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:
  • Keyboard Covers
  • Outsoles of Soccer Shoes
  • Wire and Cable
  • Airbags
  • Sheets and Film
  • Hoses and Tubing
  • Shoe Components
  • Fire Hoses

Information provided by SK Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Linear Mold Shrinkage 0.0045 cm/cm0.0045 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Hardness, Shore D 3535ASTM D2240
Tensile Strength, Ultimate 34.3 MPa4980 psiASTM D412
Elongation at Break 600 %600 %ASTM D412
100% Modulus 5.38 MPa
@Strain 100 %
780 psi
@Strain 100 %
ASTM D412
300% Modulus 12.4 MPa
@Strain 300 %
1800 psi
@Strain 300 %
ASTM D412
Resilience 4040Vertical Rebound; ASTM D2632
Tear Strength 98.1 kN/m560 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 2020H18 wheel, 1000g load; ASTM D1044
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 195 °C383 °FTransition Temperature
 195 °C383 °FMetering Temperature
Middle Barrel Temperature 190 °C374 °F
Nozzle Temperature 200 °C392 °F
Zone 1 180 °C356 °F
Zone 2 185 °C365 °F
Zone 3 190 °C374 °F
Zone 4 195 °C383 °F
Adapter Temperature 195 °C383 °F
Die Temperature 195 °C383 °FTip
 200 °C392 °FBody
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR2102-85AE Polycaprolactone Ester Polyurethane
Wanhua Chemical Wanthane® WHT-7180 Polycaprolactone Based TPU
SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based
Covestro Desmopan® 9385A TPU

PSK030 / 67765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.