MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pewter, Annealed Sheet
Categories: Metal; Nonferrous Metal; Tin Alloy

Material Notes: Modern composition range listed; pewter formerly was a lead-tin alloy but lead is no longer added because of toxicity and dullness concerns. Applications include jewelry and kitchen and home decor products such as candlesticks, mugs, plates, etc. Pewter is typically cast between 315-330°C.

Key Words: Tin Alloys
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.28 g/cc0.263 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 9.59.5
Tensile Strength, Ultimate 59.0 MPa8560 psi
Elongation at Break 40 %40 %in 50 mm
Modulus of Elasticity 53.0 GPa7690 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 244 - 295 °C471 - 563 °F
Solidus 244 °C471 °F
Liquidus 295 °C563 °F
 
Processing PropertiesMetricEnglishComments
Casting Temperature 315 - 330 °C599 - 626 °Ftypical
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb 1.0 - 8.0 %1.0 - 8.0 %
Copper, Cu 0.25 - 3.0 %0.25 - 3.0 %
Lead, Pb <= 0.50 %<= 0.50 %
Tin, Sn 90 - 98 %90 - 98 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pewter, Cold-Rolled Sheet
Pewter, Britannia Metal
Tin, ASTM B 23 Babbitt Alloy 1 (White Metal)
Tin, ASTM B 23 Babbitt Alloy 2 (UNS L13890)
68.4Pb-30Sn-1.6Sb Tin-Lead-Antimony Solder, ASTM Class 30C

MLT000 / 12281

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.