MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffness

Applications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert and conduit application

Additives: Antioxidants and processing stabilizers

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9535 g/cc0.03445 lb/in³ASTM D792
ESCR 10% Igepal® >= 75 hour
@Temperature 50.0 °C
>= 75 hour
@Temperature 122 °F
F0-; ASTM D1693
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Yield 27.0 MPa3920 psiExtension rate 2 in/min; ASTM D638
Elongation at Break >= 900 %>= 900 %Extension rate 2 in/min; ASTM D638
Flexural Modulus 1.24 GPa180 ksiTangent; ASTM D790
 1.035 GPa
@Strain 2 %
150.1 ksi
@Strain 2 %
Secant; ASTM D3350
 
Thermal PropertiesMetricEnglishComments
CTE, linear 140 µm/m-°C
@Temperature 20.0 °C
77.8 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 132 °C270 °FASTM D3417
Maximum Service Temperature, Air 264 °C507 °FASTM D3350
Vicat Softening Point 126 °C259 °FASTM D1525
Brittleness Temperature <= -70.0 °C<= -94.0 °FF0 notched specimen; ASTM D746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 175 - 220 °C347 - 428 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
Ipiranga Petrochem GF 5150 HDPE
Ineos TUB 121 HDPE
Ineos CP52-35 HDPE
Ineos B53-35H-124 Blow Molding Grade Polyethylene

PNOVA122 / 55023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.