MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxy Technology EPO-TEK® B9021-1 Epoxy Paste
Categories: Polymer; Thermoset; Epoxy

Material Notes: Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate attach. For opto-packaging, it can be used as the main gasket seal of glass plates in LCDs, or for sealing filter windows onto optosensors. A more thixotropic and viscous version of EPO-TEK® B9021.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/cc
Particle Size <= 20 µm<= 20 µm
Viscosity 10000 - 15000 cP
@Temperature 23.0 °C
10000 - 15000 cP
@Temperature 73.4 °F
50 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474
Tensile Modulus 1.40 GPa203 ksiStorage
Shear Strength >= 9.38 MPa>= 1360 psiDie
 9.984 MPa1448 psiLap
 
Thermal PropertiesMetricEnglishComments
CTE, linear 97.0 µm/m-°C53.9 µin/in-°FBelow Tg
 145 µm/m-°C80.6 µin/in-°FAbove Tg
Maximum Service Temperature, Air 150 °C302 °FContinuous
 250 °C482 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 50.0 °C>= 122 °F
Decomposition Temperature 307 °C585 °FDegradation Temperature
 
Processing PropertiesMetricEnglishComments
Dry Time <= 24.0 hour<= 24.0 hour
Cure Time 30.0 min
@Temperature 75.0 °C
0.500 hour
@Temperature 167 °F
minimum, B-stage
Pot Life 40320 min40320 min
Shelf Life 12.0 Month12.0 Monthrefrigerated
 
Descriptive Properties
ColorCreambefore cure
ConsistencySmooth Thixotropic paste
Number of ComponentsSingle
Weight Loss3.37%200°C
 4.22%250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® OG142 UV Cure Optical Epoxy

PPOXYT155 / 141194

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.