MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NYCOA 5100 HS Heat Stabilized, Impact Modified Nylon 66 Resin
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: NYCOA 5100 HS is an impact modified, heat stabilized Nylon 66 resin used for injection molding. This material is specially formulated to provide improved flexibility and ductility vs standard Nylon 66.

NYCOA 5100 HS offers outstanding toughness, exceptional processability, and a greater service life at elevated temperatures than standard grades of Nylon 66. It is available in UV stable, and custom colors grades. It also has excellent chemical resistance to greases, oils, and other hydrocarbons.

Typical applications include automotive wiring harnesses, motor component housings, gears, and electrical connectors.

Information provided by Nycoa, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792
Water Absorption 1.2 %1.2 %24 hours; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Yield 65.0 MPa9430 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Flexural Strength 85.0 MPa12300 psiASTM D790
Flexural Modulus 2.22 GPa322 ksiASTM D790
Izod Impact, Notched 1.35 J/cm2.53 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 258 °C496 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 189 °C372 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo EMERGE™ 5100 Acrylonitrile Butadiene Styrene (ABS)
EMS-Griltech Grilon® TM 5100 White Nylon 6 Fiber
RTP Company RTP 1400 R-5100 Polyphenylsulfone (PPSU)
Dow UCON™ 50-HB-5100 PAG Lubricant
Dow Elite® 5100 Linear Low Density Polyethylene

PNYCO05 / 55540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.