MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epsan Eplamid 6 CFR 10 BK Q1B001 Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Polyamide 6, reinforced with 10% of carbon fiber, heat stabilized, lubricated for injection molding. Eplamid 6 CFR 10 is used in all sectors of industry, offering a perfect balance of thermal and mechanical properties.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 - 1.21 g/cc0.0426 - 0.0437 lb/in³ISO 1183
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inParallel; ISO 294-4
 0.0080 cm/cm0.0080 in/inNormal; ISO 294-4
Ash 10 %
@Temperature 550 °C,
Time 600 sec
10 %
@Temperature 1020 °F,
Time 0.167 hour
Filler by weight; Carbon Fiber
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 105 - 145 MPa15200 - 21000 psiISO 527-2
Elongation at Break 2.0 - 4.0 %2.0 - 4.0 %ISO 527-2
Tensile Modulus 6.00 - 7.00 GPa870 - 1020 ksiISO 527-2
Flexural Strength 120 - 180 MPa17400 - 26100 psiISO 178
Flexural Modulus 5.50 - 6.00 GPa798 - 870 ksiISO 178
Izod Impact, Notched (ISO) 6.00 - 9.00 kJ/m²2.86 - 4.28 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.600 - 0.900 J/cm²2.86 - 4.28 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 200 - 230 °C392 - 446 °FISO 3146
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
UL-94
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FRecommended Injection Molding Temperature
Drying Temperature 80.0 °C176 °FAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL A63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
Epsan Eplamid 6 CFR 30 BK Q1D001 Polyamide 6
Epsan Eplamid 6 GX0 15 RP BK Q1D0B501 Polyamide 6, Halogen Free
Epsan Eplamid 6 NC HV A3,6 Polyamide 6
Epsan Eplamid 66 GFI 20 NC Q1C0A801 Polyamide 66

PEPSAN003 / 186317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.