MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical Lupoy 1201-08 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Description: LUPOY PC 1201-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.

Main Characteristics: FDA, Medium Viscosity and Good mold release

Applications: Toys, Food utensils and Packaging applications

CAS: 103598-77-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
0.15 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
0.32 %
@Temperature 73.4 °F
50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm0.00050 - 0.00070 in/inASTM D955
Melt Flow 8.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
8.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7373ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Ultimate 72.0 MPa10400 psiASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi50mm/min; ASTM D638
Elongation at Break 150 %150 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.41 GPa350 ksiASTM D638
Flexural Yield Strength 96.0 MPa13900 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched 9.074 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
17.00 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy 89.0 J
@Thickness 3.20 mm
65.6 ft-lb
@Thickness 0.126 in
203m/min; ASTM D3763
Abrasion 45
@Load 1.00 kg
45
@Load 2.20 lb
[%], CS-10 F wheel, 500 cycles; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+17 ohm-cm2.00e+17 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inASTM D149
Dissipation Factor 0.0010
@Frequency 60.0 Hz
0.0010
@Frequency 60.0 Hz
ASTM D150
Comparative Tracking Index 250 V
@Thickness 2.00 mm
250 V
@Thickness 0.0787 in
IEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D696
Hot Ball Pressure Test >= 125 °C>= 257 °FIEC 598-1
Deflection Temperature at 0.46 MPa (66 psi) 144 °C
@Thickness 4.00 mm
291 °F
@Thickness 0.157 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  128 °C
@Thickness 4.00 mm
262 °F
@Thickness 0.157 in
Unannealed; ASTM D648
 141 °C
@Thickness 4.00 mm
286 °F
@Thickness 0.157 in
Annealed; ASTM D648
Vicat Softening Point 150 °C
@Load 5.10 kg
302 °F
@Load 11.2 lb
50°C/hr; ASTM D1525
Softening Point 150 - 200 °C302 - 392 °Fmelting point per MSDS
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
ASTM D635
 V-2
@Thickness 0.500 mm
V-2
@Thickness 0.0197 in
ASTM D635
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
ASTM D635
 V-2
@Thickness 2.50 - 2.70 mm
V-2
@Thickness 0.0984 - 0.106 in
ASTM D635
Flash Point >= 450 °C>= 842 °F
Oxygen Index 26 %26 %ASTM D2863
Glow Wire Test 850 °C
@Thickness 2.00 mm,
Time 5.00 sec
1560 °F
@Thickness 0.0787 in,
Time 0.00139 hour
IEC 695-2-1
Ignition Temperature >= 460 °C>= 860 °FAutoignition
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Haze 0.70 - 1.5 %0.70 - 1.5 %ASTM D1003
Transmission, Visible 89 %89 %ASTM D1003
 
Descriptive Properties
Average Extent of BurningASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupoy 1302-05 Polycarbonate Resin
LG Chemical Lupoy 1200-08 Polycarbonate Resin
LG Chemical Lupoy 1303-07 Polycarbonate Resin
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin
LG Chemical Lupoy 1201-15 Polycarbonate Resin

PLAY641 / 148651

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.