MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilon® BG-60 FC PA6-GF60
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties:
  • Short cycle times
  • Excellent surface finish
  • Easy flowing
  • Easy processing
Application examples are stressed functional parts in automotive engine compartment and housings for electro /electronic industry.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.69 g/cc0.0611 lb/in³Dry; ISO 1183
Water Absorption 4.2 %4.2 %Sim. to ISO 62
Moisture Absorption 1.10 %1.10 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 156 MPa22600 psiConditioned; ISO 2039-1
 273 MPa39600 psiDry; ISO 2039-1
Tensile Strength at Break 160 MPa23200 psiConditioned; ISO 527-1/-2
 245 MPa35500 psiDry; ISO 527-1/-2
Elongation at Break 3.2 %3.2 %Dry; ISO 527-1/-2
 3.4 %3.4 %Conditioned; ISO 527-1/-2
Tensile Modulus 13.5 GPa1960 ksiConditioned; ISO 527-1/-2
 19.0 GPa2760 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 9.10 J/cm²
@Temperature 23.0 °C
43.3 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 9.60 J/cm²
@Temperature 23.0 °C
45.7 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 2.60 J/cm²
@Temperature 23.0 °C
12.4 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cm1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 33.0 kV/mm838 kV/inConditioned; IEC 60243-1
 36.0 kV/mm914 kV/inDry; IEC 60243-1
Comparative Tracking Index 475 V475 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C7.78 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-1/-2
Melting Point 223 °C433 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 130 - 150 °C266 - 302 °FLong Term; ISO 2578
 200 °C392 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 190 °C374 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveInterior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
FormGranules
Industry & Consumer goodsHousewares
 Mechanical Engineering
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesImproved flowability and demolding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sinotek Materials BG Board Ceramic Fiber Board, White, Heat Insulation Material
Celanese Celstran® PA6-GF60-01 Nylon 6, 60% Glass Reinforced
EMS-Grivory Grilamid® XE 4106 nat PA612-GF30
LG Chemical LUMID HM2604AW PA6+GF60%
Celanese Celstran® PA6-GF60-03 PA6, 60% Glass Reinforced

PGRH187 / 156896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.