MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

European Hornbeam Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Diffuse-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.

Key Words: Carpinus betulus; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.820 g/cc0.0296 lb/in³Air Dry (12-15% Moisture Content)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 7600 N1710 lb (f)Side
Tensile Strength, Ultimate 3.80 MPa551 psiPerpendicular to Grain
 153 MPa22200 psiAxial
Modulus of Rupture 0.140 GPa20.3 ksiStatic Bending
Flexural Modulus 14.7 GPa2130 ksiStatic Bending
Compressive Strength 16.7 MPa2420 psiPerpendicular to Grain
 54.0 MPa7830 psiParallel to Grain
Shear Strength 16.9 MPa2450 psiOrientation Unknown
Toughness 33.2 J24.5 ft-lb2 cm x 2 cm sample
Cleavage 10.2 kN/m58.2 lb/in
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.50 %0.50 %Axial; Green to Zero Moisture
 6.8 %6.8 %Radial; Green to Zero Moisture
 11.5 %11.5 %Tangential; Green to Zero Moisture
 19.7 %19.7 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
European Plane Wood
European Poplar Wood
European Bastralocus Wood
European Cherry Wood
European Elm Wood

PTSE080 / 71317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.