MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saxonburg Ceramics L-5 Steatite  (discontinued **)
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Steatite Ceramics exhibit excellent electrical properties.

Applications: Heater and Appliance Industries

Information provided by Saxonburg Ceramics

Effective March 12th, 2007, Du-Co Ceramics Company has acquired the assets of Saxonburg Ceramics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.70 g/cc0.0975 lb/in³
Porosity 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.5 MPa9500 psi
Flexural Strength 143 MPa20800 psi
Compressive Strength 541 MPa78500 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  800000 ohm-cm
@Temperature 900 °C
800000 ohm-cm
@Temperature 1650 °F
 5.00e+6 ohm-cm
@Temperature 700 °C
5.00e+6 ohm-cm
@Temperature 1290 °F
 3.20e+8 ohm-cm
@Temperature 500 °C
3.20e+8 ohm-cm
@Temperature 932 °F
 4.20e+9 ohm-cm
@Temperature 100 °C
4.20e+9 ohm-cm
@Temperature 212 °F
 1.30e+10 ohm-cm
@Temperature 300 °C
1.30e+10 ohm-cm
@Temperature 572 °F
 4.70e+10 ohm-cm
@Temperature 20.0 °C
4.70e+10 ohm-cm
@Temperature 68.0 °F
Dielectric Constant  7.2
@Frequency 1e+6 Hz
7.2
@Frequency 1e+6 Hz
 7.2
@Frequency 1e+7 Hz
7.2
@Frequency 1e+7 Hz
Dielectric Strength 9.06 kV/mm230 kV/in
Dissipation Factor  0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
 0.0013
@Frequency 1e+7 Hz
0.0013
@Frequency 1e+7 Hz
Dielectric Loss Index  0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
 0.010
@Frequency 1e+7 Hz
0.010
@Frequency 1e+7 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C
@Temperature 25.0 - 700 °C
4.44 µin/in-°F
@Temperature 77.0 - 1290 °F
Thermal Conductivity 2.51 W/m-K17.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1260 °C2300 °F
 
Descriptive Properties
Te Value, °C815

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sapco C 220 Steatite
Sapco C 221 Steatite
Morgan Advanced Ceramics Frequentite 1000 Steatite
Saxonburg Ceramics S-405 Cordierite
Fujipoly Industries Sarcon® 30GHR Thin-Film GHR

CSAXON04 / 1978

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.