MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond MasterSil 156 Two Part, Low Viscosity Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance, commendable flexibility and appealing thermal conductivity along with meeting UL 94V-0 for flame retardancy. MasterSil 156 is an addition cured system and does not require exposure to air for complete cross-linking. It has a convenient one to one mix ratio by weight and will not outgas while curing. It is 100% solids and contains no solvents. MasterSil 156 has a lower viscosity and excellent flow properties enabling it to be well suited for potting and encapsulation. Additionally, the electrical insulation properties are good and it still is a reputable thermal conductor. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics and many rubbers and plastics. Its flexibility allows it to withstand severe thermal cycling and resist vibration and shock. Also, it is very resistant to water, humidity, oils and environmental elements. The system is rated to 105°C by UL in thicknesses up to 1/4 inch and above, and it is listed as 94V-0 for flame retardancy. It can cure in thicknesses well beyond 1-2 inches if required. MasterSil 156 is a system that combines flexibility, high temperature resistance, heat dissipation and flame retardancy.

Product Advantages:

  • Convenient one to one by weight mix ratio
  • Addition cured; virtually no by-products released during curing; does not require air
  • Favorable electrical insulation and thermal conduction properties
  • Lower viscosity and splendid flow; ideal for potting and encapsulation
  • Very low shrinkage upon cure
  • UL flame retardant 94V-0 rating
Key Features
  • Good thermal conductivity
  • Good electrical insulation properties
  • Flame retardant UL 94V-0
  • Low exotherm; very long pot life
  • Can cure in thicknesses up to and beyond 1-2 inches
  • UL temperature rated up to 105°C

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 8000 - 12000 cP8000 - 12000 cPPart B
 15000 - 25000 cP15000 - 25000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 50 - 6050 - 60
Tensile Strength at Break 2.07 - 2.76 MPa300 - 400 psi
Elongation at Break 120 - 150 %120 - 150 %
Shear Strength >= 1.24 MPa>= 180 psiTensile lap, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.9
@Frequency 60 Hz,
Temperature 25.0 °C
3.9
@Frequency 60 Hz,
Temperature 77.0 °F
Dielectric Strength 17.7 kV/mm
@Thickness 3.17 mm
450 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 - 140 µm/m-°C61.1 - 77.8 µin/in-°F
Thermal Conductivity 1.15 - 1.30 W/m-K8.00 - 9.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
 2880 - 4320 min
@Temperature 23.9 °C
48.0 - 72.0 hour
@Temperature 75.0 °F
Pot Life 1.0 - 3.0 min1.0 - 3.0 min100 gram batch
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1:1by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV6428 Dark Gray General Purpose Potting/Encapsulating Compound
Overview of materials for Silicone Rubber
Dow 3-6751 THERMALLY CONDUCTIVE ADHESIVE, KIT
Momentive Performance Materials RTV627 Dark Gray General Purpose Potting/Encapsulating Compound
Momentive Performance Materials TSE3331 Dark Gray Thermally Conductive Potting/Encapsulating Compound

PMASTB336 / 149583

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.