MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Saflex® HP Interlayer
Material Notes:

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 23.5 MPa>= 3410 psiJIS K6771
Elongation at Break >= 190 %>= 190 %JIS K6771
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 2.19 J/g-°C
@Temperature 40.0 - 80.0 °C
0.523 BTU/lb-°F
@Temperature 104 - 176 °F
ASTM E1269
Thermal Conductivity 0.200 W/m-K
@Temperature 32.0 - 90.0 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 89.6 - 194 °F
ASTM D5930
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4881.488
 
Descriptive Properties
Emissivity0.9419.5°C, ASTM C1371

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Saflex® 0.030 inch Clear Protective Interlayer PVB Film for Glass Laminates
Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer
Trinseo Plexiglas® V825 Acrylic
Overview of materials for Polycarbonate, Extruded
Overview of materials for Cyclo Olefin Polymer

PEAT7019 / 183587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.