MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 218 V50 Black 21N PA 66 50% Glass Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYL® A 218 V50 Black 21N is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.

Key Properties: Mechanical performance; Heat stabilized

Benefits: The product offers an excellent combination between thermal and mechanical properties.

Applications: It is used in a wide variety of industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183/A
Water Absorption 0.60 %
@Time 86400 sec
0.60 %
@Time 24.0 hour
ISO 62
Viscosity  28 cP
@Shear Rate 10000 1/s,
Temperature 300 °C
28 cP
@Shear Rate 10000 1/s,
Temperature 572 °F
 30 cP
@Shear Rate 10000 1/s,
Temperature 290 °C
30 cP
@Shear Rate 10000 1/s,
Temperature 554 °F
 30.1 cP
@Shear Rate 10000 1/s,
Temperature 280 °C
30.1 cP
@Shear Rate 10000 1/s,
Temperature 536 °F
 300 cP
@Shear Rate 100 1/s,
Temperature 300 °C
300 cP
@Shear Rate 100 1/s,
Temperature 572 °F
 320 cP
@Shear Rate 100 1/s,
Temperature 290 °C
320 cP
@Shear Rate 100 1/s,
Temperature 554 °F
 400 cP
@Shear Rate 100 1/s,
Temperature 280 °C
400 cP
@Shear Rate 100 1/s,
Temperature 536 °F
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0044 cm/cm0.0044 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 220 MPa31900 psiASTM D638
 240 MPa34800 psiISO 527 Type 1A
Tensile Stress at Strain  80.0 MPa
@Strain 1.5 %
11600 psi
@Strain 1.5 %
 200 MPa
@Strain 1.5 %
29000 psi
@Strain 1.5 %
Elongation at Break 2.0 %2.0 %ISO 527 Type 1A
Tensile Modulus 16.2 GPa2350 ksiISO 527 Type 1A
Flexural Strength 350 MPa50800 psiASTM D790
Flexural Modulus 13.5 GPa1960 ksiISO 178
 13.8 GPa2000 ksiASTM D790
Izod Impact, Unnotched 0.184 J/cm0.345 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 14.5 kJ/m²6.90 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 9.50 J/cm²45.2 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²7.61 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohm6.00e+14 ohmIEC 60093
Dielectric Constant 3.73.7IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inIEC 60243
Dissipation Factor 0.0100.010IEC 60250
Comparative Tracking Index 600 V600 VSol A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
8.33 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FISO 75/Af
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
ISO 1210
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
ISO 1210
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
ISO 1210
Oxygen Index 23 %23 %ISO 4589
Glow Wire Test  650 °C
@Thickness 0.800 mm
1200 °F
@Thickness 0.0315 in
Flammability Index; ISO 60695-2-12
 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
Flammability Index; ISO 60695-2-12
 700 °C
@Thickness 3.20 mm
1290 °F
@Thickness 0.126 in
Flammability Index; ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 280 °C518 - 536 °FCompression zone
 280 - 290 °C536 - 554 °FMixing zone
Feed Temperature 265 - 275 °C509 - 527 °F
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Dry
Domo TECHNYL® A 218 V50 Black 21N PA 66 50% Glass Reinforced, Conditioned

PSOLVAY836 / 218564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.