MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucobit Lucolast® 7010 Ethylene Butyl Acrylate Asphalt Additive
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Lucolast® 7010 is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Addition of Lucolast 7010 to bitumen increases its viscosity, broadens the range of plasticity, and displays significant advantages in improving resistance to deformation.

Information provided by Lucobit AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³
 1.00 - 1.10 g/cc0.0361 - 0.0397 lb/in³2.4% Lucolast in Bitumen B50/70
Apparent Bulk Density 0.500 g/cc0.0181 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 860 %860 %
Modulus of Elasticity 0.0620 GPa8.99 ksi
 
Thermal PropertiesMetricEnglishComments
Softening Point 80.0 - 100 °C176 - 212 °F
Brittleness Temperature <= -30.0 °C<= -22.0 °F
Ring & Ball Softening Point >= 55.0 °C>= 131 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucobit Lucocell® FG3000 Cellulose Asphalt Additive
Honeywell Titan™ 7205 Polymers for Asphalt Modification
ELM® Concrete/Asphalt WS Biodegradable Form Release Agent
Asphalt

PLUCO954 / 151020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.