MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Applications
Microthene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh powder and is also available in pellet form Petrothene GA574189.

Regulatory Status
MP574189 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520.

Processing Techniques
Specific recommendations for processing MP574189 can only be made when the processing conditions, equipment and end use are known.

Key Words: FDA 21 CFR 177.1520.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ASTM D1505
Melt Flow 50 g/10 min50 g/10 minASTM D1238
Spiral Flow 45.5 cm17.9 inEquistar
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength at Break 8.96 MPa1300 psi20 in/min; ASTM D638
Tensile Strength, Yield 15.2 MPa2200 psi20 in/min; ASTM D638
Elongation at Yield 11 %11 %20 in/min; ASTM D638
Flexural Modulus, 1% Secant 483 MPa70000 psi0.5 in/min; ASTM D790
2% Secant Modulus 0.421 GPa61.0 ksi0.5 in/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 47.2 °C117 °FASTM D648
Vicat Softening Point 84.4 °C184 °FASTM D1525
Brittleness Temperature -72.2 °C-98.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 °C350 °F
Middle Barrel Temperature 191 °C375 °F
Front Barrel Temperature 204 °C400 °F
Nozzle Temperature 204 °C400 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Purell GA7760 High Density Polyethylene (HDPE), Injection Molded
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500

PEQU0853 / 157474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.