MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Albis Plastics Polypropylene A 13 H-BS 73 , 73% Barium Sulfate Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Semi-crystalline Polypropylene Homopolymer (PPHP)

Characteristics: Highly Filled: High Density, Good X-ray Contrast Characteristics

Applications: Ballast Material for Vertical Blinds

Processing: Injection Molding (Melt Temperature: 425-575°F, Mold Temperature: 65-160°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³DIN 53 479
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
DIN 53 735
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 15.0 MPa2180 psiDIN 53 455
Modulus of Elasticity 2.00 GPa290 ksiDIN 53 457
Flexural Yield Strength 25.0 MPa3630 psiDIN 53 452
Izod Impact, Notched 0.500 J/cm0.937 ft-lb/inDIN 53 453
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C147 °FDIN 53 461
Vicat Softening Point 50.0 °C122 °F(VST/B/50); DIN 53 460
 
Processing PropertiesMetricEnglishComments
Melt Temperature 218 - 302 °C424 - 576 °FInjection
Mold Temperature 18.0 - 71.0 °C64.4 - 160 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman JPP60BX03NA 60% Barium Sulfate Filled, Heat-Stabilized, Homopolymer Polypropylene
A. Schulman JPP60BX02BK 60% Barium Sulfate Filled, Heat-Stabilized, Homopolymer Polypropylene containing 25% P.C.R.
Overview of materials for Polypropylene, Mineral Reinforced
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Plastics Group Polifil® BS-70 70% Barium Sulfate Reinforced Polypropylene

PZA1B98 / 21785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.