MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BCC Products BC 7009-2 Epoxy Casting
Categories: Polymer; Thermoset; Epoxy

Material Notes: BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in metal or conductive-type molds can successfully be achieved as well. Ideal for stretch forms, patterns, dies, molds, duplications, prototypes, etc.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.27 g/cc2.27 g/cc
Brookfield Viscosity 35000 cP
@Temperature 23.9 °C
35000 cP
@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.00090 cm/cm0.00090 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85
@Temperature 23.9 °C
85
@Temperature 75.0 °F
Tensile Strength, Ultimate 37.2 MPa5400 psi
Flexural Strength 51.0 MPa7400 psi
Flexural Modulus 5.58 GPa810 ksi
Compressive Strength 86.9 MPa12600 psi
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C123 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 24.0 °C
24.0 hour
@Temperature 75.2 °F
Pot Life 240 min
@Temperature 24.0 °C
240 min
@Temperature 75.2 °F
15 lb. mass
 
Descriptive Properties
MachinabilityGood
Mix Ratio12:1 by weight, 4.5:1 by volume, resin/harder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products BC 7009-1 Epoxy Casting
7009 Aluminum Composition Spec
Alcoa 7055-T77511 Aluminum Extrusions
Lotte Advanced Materials Infino® CA-7009 PA/PPE, Antistatic
KaMin Nucote® 7009 Kaolin Clay - Surface Treated

PBCC033 / 107260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.