MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Johnson Matthey Nickelbraze™ HTN3 Nickel Based Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Nickel Alloy; Solder/Braze Alloy

Material Notes: Nickelbraze™ HTN brazing filler metals are used to join stainless steel, nickel and cobalt base alloys. They provide exceptional resistance to chemical corrosion and oxidation coupled with high strength at elevated temperatures. These alloys are widely used particularly within the aerospace, automotive and nuclear industries using vacuum or controlled atmosphere brazing methods.

These products are available as pastes, powders or tapes. Several can be supplied in rapidly solidified foil form.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 980 - 1040 °C1800 - 1900 °F
Solidus 980 °C1800 °F
Liquidus 1040 °C1900 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 3.1 %3.1 %
Iron, Fe 0.50 %0.50 %
Nickel, Ni 91.9 %91.9 %
Silicon, Si 4.5 %4.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey Nickelbraze™ HTN7 Nickel Based Brazing Filler Metal
Kennametal Stellite Deloro® 55 Nickel Alloy
Kennametal Stellite Nucalloy® 488V High-Silicon Nickel-Base Hardfacing Alloy
Johnson Matthey Nickelbraze™ HTN1 Nickel Based Brazing Filler Metal
Johnson Matthey Nickelbraze™ HTN4 Nickel Based Brazing Filler Metal

NJMMJ9880 / 186281

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.