MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 2000 Phenolic, Granular, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Woodflour Filled

Material Notes: PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under component file E40654. 02000 is available in black.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.630 g/cc0.0228 lb/in³ASTM D1895
Density 1.39 g/cc0.0502 lb/in³ASTM D792
Water Absorption 0.40 %0.40 %ASTM D570
Linear Mold Shrinkage 0.0044 cm/cm0.0044 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 9090ASTM D785
Tensile Strength, Ultimate 51.0 MPa7400 psiASTM D638
Elongation at Break 0.65 %0.65 %ASTM D638
Tensile Modulus 8.60 GPa1250 ksiASTM D638
Flexural Strength 92.0 MPa13300 psiASTM D790
Flexural Modulus 8.10 GPa1170 ksiASTM D790
Compressive Strength 212 MPa30700 psiASTM D695
Izod Impact, Notched 0.174 J/cm0.326 ft-lb/inASTM D256
Charpy Impact, Notched 0.187 J/cm²0.890 ft-lb/in²ASTM D256
Impact 109109J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.20e+11 ohm-cm3.20e+11 ohm-cmASTM D247
Dielectric Constant 5.25.2ASTM D150
Dielectric Strength 12.2 kV/mm310 kV/inShort Time; ASTM D149
Dissipation Factor 0.0520.052ASTM D150
Arc Resistance 132 sec132 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.0 µm/m-°C
@Temperature 40.0 - 130 °C
32.8 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.390 W/m-K
@Temperature 100 °C
2.71 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 207 °C405 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 176 °C349 °FASTM D648
Flammability, UL94 V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
Oxygen Index 27.9 %27.9 %ASTM D2863
Shrinkage 0.203 %0.203 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 2571 Phenolic, Granular, Compression Molded
Cookson Group Plaskon® 440 Mineral Filled Novolac Epoxy Molding Compound
Plenco 1501 Polyester, Briquette, Transfer Molded
Cookson Group Plaskon® 3100 Novolac Epoxy Molding Compound
Plenco 2300 Phenolic, Granular, Compression Molded

PLEL32 / 50600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.