MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Devcon Wear Guard (High Temp) Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Abrasion-Resistant System

Comments: Putty

Data provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.83 g/cc0.0662 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787ASTM D2240
Tensile Strength, Ultimate 31.7 MPa4600 psiASTM D638
Tensile Modulus 5.86 GPa850 ksiASTM D638
Flexural Yield Strength 56.7 MPa8220 psiASTM D790
Compressive Yield Strength 91.0 MPa13200 psiASTM D695
Adhesive Bond Strength 15.9 MPa2300 psiAdhesive tensile shear strength; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3838ASTM D150
Dielectric Strength 12.2 kV/mm310 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 49.0 µm/m-°C
@Temperature 20.0 °C
27.2 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.895 W/m-K6.20 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 232 °C450 °FOperating Temperature
Shrinkage 0.10 %0.10 %During Cure; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Processing Temperature 21.1 °C70.0 °F
Pot Life 120 min
@Temperature 23.9 °C
120 min
@Temperature 75.0 °F
 
Descriptive Properties
Coverage per lb.60 in²at 1/4 inch thick
Mix Ratio by Volume6 to 1resin:hardener
Mix Ratio by Weight13.7 to 1resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armstrong A-661 Epoxy Adhesive
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

PITWX21 / 48508

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.