MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPC 4720 WZ Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 4720 is an impact copolymer. 4720 is characterized by a high fluidity offering a combination of east of processing and good mechanical properties.

Application

ATOFINA 4720 has been formulated for the manufacture of thin-walled containers and household articles.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 25 g/10 min25 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.5 MPa3700 psiASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus 1.31 GPa190 ksiASTM D 790
Izod Impact, Notched 1.00 J/cm1.87 ft-lb/inASTM D256
 0.400 J/cm
@Temperature -20.0 °C
0.749 ft-lb/in
@Temperature -4.00 °F
ASTM D256
Charpy Impact Unnotched 0.900 J/cm²4.28 ft-lb/in²Notched/Unnotched not specified; ASTM DIN53453
 0.400 J/cm²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
Notched/Unnotched not specified; ASTM DIN53453
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FASTM D648
Vicat Softening Point 148 °C298 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 3720WZ Polypropylene, Injection Molding Grade
Flint Hills P5M6K-080 Polypropylene Random Copolymer
Flint Hills AP5325-HS Impact Copolymer Polypropylene
Flint Hills P5L2K-055 Polypropylene Random Copolymer
Total PPH 3620WZ Polypropylene, Injection Molding Grade

PFINAA072 / 38508

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.