MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene® LD 720.01 Specialty Film Resin
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and toughness. These resins are also used in specialized molding applications.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 10000 ppm
  • Slip: 7050 ppm
  • Thermal Stabilizer: Yes
Applications:
  • Heat Seal Layer
  • Injection Molding
  • Shoe Soles

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.941 g/cc0.0340 lb/in³ExxonMobil Method
Vinyl Acetate Content 18.5 %18.5 %ExxonMobil Method
Melt Flow 1.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ExxonMobil Method
Antiblock Level 10000 ppm10000 ppm
Slip Level 7050 ppm7050 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 180 %180 %ASTM D882
Film Elongation at Break, TD 650 %650 %ASTM D882
Elmendorf Tear Strength MD 40 g40 gASTM D1922
Elmendorf Tear Strength TD 80 g80 gASTM D1922
Dart Drop Test 370 g0.816 lbASTM D1709A
Film Tensile Strength at Break, MD 26.9 MPa3900 psiASTM D882
Film Tensile Strength at Break, TD 27.6 MPa4000 psiASTM D882
1% Secant Modulus, MD 65.5 MPa9500 psiASTM D882
1% Secant Modulus, TD 68.9 MPa10000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 86.1 °C187 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 62.2 °C144 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 28 %28 %ASTM D1003
Gloss 49 %49 %45°C; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Elevate™ EB591 9% EVA Copolymer
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion)
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion)
Dow ELITE™ 5500G Enhanced Polyethylene Resin

PEXB145 / 37450

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.