MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Alloy M65 (C17465) Beryllium Copper Rod  (discontinued **)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Alloy M65 (C17465) is a machinable, high-performance, copper beryllium rod alloy from Brush Wellman. M65 has excellent strength, conductivity, and resistance to elevated temperature stress relaxation. The machinability of M65 is 80% of free machining brass. M65 is pre-hardened - No heat treatment is required after machining.

Information supplied by Brush Wellman Engineered Materials.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 2424
Hardness, Vickers 260260
Tensile Strength, Ultimate >= 896 MPa>= 130000 psi
Tensile Strength, Yield >= 827 MPa>= 120000 psi
Elongation at Break 8 %8 %
Modulus of Elasticity 138 GPa20000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000382 ohm-cm0.00000382 ohm-cmConductivity is 45% IACS
Magnetic Permeability 0.999970.99997
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 225 W/m-K1560 BTU-in/hr-ft²-°F
Melting Point 1030 °C1880 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.20 - 0.50 %0.20 - 0.50 %
Copper, Cu 97.5 - 98.6 %97.5 - 98.6 %As remainder
Lead, Pb 0.20 - 0.60 %0.20 - 0.60 %
Nickel, Ni 1.0 - 1.4 %1.0 - 1.4 %
 
Descriptive Properties
Machinability (% of C36000)80%
Stress Relaxation72%at 200°C for 1000 hr
 81%at 175°C for 1000 hr
 86%at 150°C for 1000 hr
 90%at 125°C for 1000 hr

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phosphor bronze 5% Sn, UNS C51000
Ampco Metal AMPCOLOY® 89 Beryllium Copper, Extrusion
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17500)
Beryllium Copper, UNS C17000
Brush Wellman Beryllium-Copper Alloy 171 1/4 HT (TH01) Temper

NBBC15 / 15325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.