MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow AFFINITY™ EG 8100G Ethylene-octene copolymer
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: AFFINITY™ EG 8100G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene-octene copolymer exhibiting high flexibility and elasticity. It can be utilized in monolayer and coextruded films and in blends with other polyolefins to enhance clarity, sealability and toughness of the structure.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc0.0314 lb/in³ASTM D792
Mooney Viscosity 23.6
@Temperature 121 °C
23.6
@Temperature 250 °F
ML 1+4; ASTM D1646
Melt Flow 1.0 g/10 min1.0 g/10 minMelt Flow Ratio = 7.6 (I10/I2); ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7474ASTM D2240
Tensile Strength, Ultimate 10.60 MPa1537 psiASTM D638
Tensile Strength, Yield 1.71 MPa248 psiASTM D638
 6.12 MPa887 psi100% Secant; ASTM D638
Elongation at Break 1115 %1115 %ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 55.0 °C131 °FDow Method
Vicat Softening Point 42.8 °C109 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ PL 1840G Polyolefin Plastomer (POP)
Dow AFFINITY™ EG 8100 Polyolefin Elastomer
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP)
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer

PDOW1164 / 30382

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.