MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem H521 Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: Injection Molding, General Purpose, Low Water Carryover

Applications: Suggested Uses Include Tape, Slit-film Fibers, Containers, Closures, Housewares

This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 3.6 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.6 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ASTM D785
Tensile Strength 37.2 MPa5400 psi2 in/min; ASTM D638
Elongation at Yield 10 %10 %2 in/min; ASTM D638
Tenacity 0.397 N/tex4.50 g/denier3.3 draw ration, 1,250 m/min roll speed; 225°C spin temperature, D1000/68, ASTM D2256
Flexural Modulus, 1% Secant 1650 MPa240000 psi0.05 in/min; ASTM D-790A
Izod Impact, Notched 0.374 J/cm0.700 ft-lb/inASTM D256A
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Elongation of Fibers (3.3 draw ration, 1,250 m/min roll speed)36%225°C spin temperature, D1000/68, ASTM D2256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Flint Hills PP 23R2A Random Copolymer Polypropylene
A. Schulman ComAlloy Aqualoy® 125 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL
Omni Plastics OmniPro™ HPP GRC40 Homopolymer Polypropylene, 40% Glass reinforced
Omni Plastics OmniPro™ HPP TF40 Homopolymer Polypropylene, 40% Talc reinforced

PBRASK066 / 133704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.