MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Water Absorption 5.2 - 5.8 %5.2 - 5.8 %ISO 62
Moisture Absorption at Equilibrium 1.5 - 1.9 %1.5 - 1.9 %23°C/50% R.H.; ISO 62
Viscosity Number 145 cm³/g1.45 dl/g
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/in
Melt Flow 54.4 g/10 min
@Load 5.00 kg,
Temperature 275 °C
54.4 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 190 MPa27600 psiISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Modulus of Elasticity 10.0 GPa1450 ksi
Flexural Strength 280 MPa40600 psiiso 178
Flexural Modulus 8.60 GPa1250 ksiISO 178
Izod Impact, Notched (ISO) 11.5 kJ/m²5.47 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 8.50 J/cm²40.5 ft-lb/in²ISO 179/1eU
 7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 V550 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
11.1 - 16.7 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359
CTE, linear, Transverse to Flow 60.0 - 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
33.3 - 38.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°F
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FDIN 52612
Melting Point 260 °C500 °FDIN 53765
Maximum Service Temperature, Air 135 °C275 °Ffor 50% loss of tensile strength after 20,000 hr
 165 °C329 °Ffor 50% loss of tensile strength after 5,000 hr
 240 °C464 °FISO 527
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 80.0 - 90.0 °C176 - 194 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1500
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned)
Overview of materials for Nylon 66, 30% Glass Fiber Filled
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Dry)
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Dry)

PBASF9221 / 84985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.