MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical Lupox® TE5006F PET+PC  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTI

Application: IT/OA, E&E (Connector)

CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm
@Thickness 3.20 mm
0.0060 - 0.010 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 58.8 MPa
@Thickness 3.20 mm
8530 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break >= 100 %
@Thickness 3.20 mm
>= 100 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 88.3 MPa
@Thickness 3.20 mm
12800 psi
@Thickness 0.126 in
2.8mm/min; ASTM D790
Flexural Modulus 2.30 GPa
@Thickness 3.20 mm
334 ksi
@Thickness 0.126 in
2.8mm/min; ASTM D790
Izod Impact, Notched 0.588 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.10 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=0.750 mm
30 - 60 sec
@Thickness >=0.0295 in
 30 - 60 sec
@Thickness >=1.00 mm
30 - 60 sec
@Thickness >=0.0394 in
 30 - 60 sec
@Thickness >=1.60 mm
30 - 60 sec
@Thickness >=0.0630 in
 60 - 120 sec
@Thickness >=3.00 mm
60 - 120 sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 0.750 mm
>= 120 arcs
@Thickness 0.0295 in
 >= 120 arcs
@Thickness 1.00 mm
>= 120 arcs
@Thickness 0.0394 in
 >= 120 arcs
@Thickness 1.60 mm
>= 120 arcs
@Thickness 0.0630 in
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR 25.4 - 50.0 mm/min1.00 - 1.97 in/min
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F@ Break; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
@Thickness 6.40 mm
230 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical  75.0 °C
@Thickness >=0.500 mm
167 °F
@Thickness >=0.0197 in
 110 °C
@Thickness >=0.750 mm
230 °F
@Thickness >=0.0295 in
 110 °C
@Thickness >=1.00 mm
230 °F
@Thickness >=0.0394 in
 120 °C
@Thickness >=1.60 mm
248 °F
@Thickness >=0.0630 in
 120 °C
@Thickness >=3.00 mm
248 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  75.0 °C
@Thickness >=0.500 mm
167 °F
@Thickness >=0.0197 in
 110 °C
@Thickness >=0.750 mm
230 °F
@Thickness >=0.0295 in
 110 °C
@Thickness >=1.00 mm
230 °F
@Thickness >=0.0394 in
 120 °C
@Thickness >=1.60 mm
248 °F
@Thickness >=0.0630 in
 120 °C
@Thickness >=3.00 mm
248 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  75.0 °C
@Thickness >=0.500 mm
167 °F
@Thickness >=0.0197 in
 110 °C
@Thickness >=0.750 mm
230 °F
@Thickness >=0.0295 in
 110 °C
@Thickness >=1.00 mm
230 °F
@Thickness >=0.0394 in
 120 °C
@Thickness >=1.60 mm
248 °F
@Thickness >=0.0630 in
 120 °C
@Thickness >=3.00 mm
248 °F
@Thickness >=0.118 in
Flammability, UL94  V-0
@Thickness >=0.500 mm
V-0
@Thickness >=0.0197 in
 V-0
@Thickness >=0.750 mm
V-0
@Thickness >=0.0295 in
 V-0
@Thickness >=1.00 mm
V-0
@Thickness >=0.0394 in
 V-0
@Thickness >=1.60 mm
V-0
@Thickness >=0.0630 in
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
 5VB
@Thickness >=1.60 mm
5VB
@Thickness >=0.0630 in
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 260 °C482 - 500 °FInjection Molding
Middle Barrel Temperature 260 - 270 °C500 - 518 °FInjection Molding
Front Barrel Temperature 260 - 270 °C500 - 518 °FInjection Molding
Nozzle Temperature 260 - 270 °C500 - 518 °FInjection Molding
Melt Temperature 260 - 270 °C500 - 518 °FInjection Molding
Mold Temperature 40.0 - 80.0 °C104 - 176 °FInjection Molding
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hourInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Envalior Pocan® C 1206 000000 PET+PC
Star Plastics PC/PET7901 Molding Grade PC/PET
Mitsubishi Iupilon® MB 2105 PC/Polyester
LG Chemical LUPOX TE5006FH PET+PC, Injection Molding

PLAY348 / 148358

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.