MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

M Chemical GUARD DOG™ UV1577 Light Absorber, Triazene Derivative
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GUARD DOG™ UV1577 UV absorber is a low volatile Triazine based UV absorber which is highly effective in polymers that are processed at high temperature (decomposition temperature > 350°C).

Applications: Extremely effective in PP, SBS, footwear, SEBS, acetal, acrylic, PET, PMMA, PBT, PC and is recommended for thin section and fiber applications suitable for food contact applications.

Performance Benefits:

  • Strong absorption of UV radiation in the 300 - 400 nm regions
  • Low initial color and low volatility during high processing temperatures and have good extraction resistance.

Typical Properties:

  • Free flowing, pale yellow powder
  • Solubility (g/100ml @ 20°C): Acetone 2, Benzene 10, CHCl3 35, MeCl 34, MEK 13, Toluene 20

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
Molecular Weight 425.52 g/mol425.52 g/mol
Vapor Pressure 2.00e-15 bar1.50e-12 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point 147 - 151 °C297 - 304 °F
Flash Point >= 150 °C>= 302 °FIgnition
 
Descriptive Properties
CAS Number147315-50-2
Molecular FormulaC27H27N3O2
Name2-(4, 6-diphenyl-1, 3,5-triazin-2-yl)-5-[(hexyl)oxy]phenol
Purity (%)>98by HPLC
Recommended Dosage0.15 - 0.60%depending upon the substrate and performance requirements

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oceanchem Group Melamine Polyphosphate (MPP)
Arkema LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate
Chengdu Polyster RPM540B Flame Retardant Masterbatch
M Chemical GUARD DOG™ UV234 Light Absorber, Benzotriazole Derivative
Lanxess STABAXOL® KE 9193 Masterbatch Antihydrolysis agent

PMCHEM904 / 135143

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.