MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ethydco Advancene™ EM-5420-AAH High Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: A high density polyethylene resin is produced via advanced gas phase PE process and is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. This resin has been designed to provide an excellent balance of toughness, environmental stress crack resistance and processability. Main characteristics: for injection molded housewares, toys, food containers and pails. Excellent balance of toughness, stress crack resistance and processability. Hexene high density resin. Very narrow molecular weight distribution.

Mechanical property data for samples molded and tested in accordance with ASTM D4976.

Information provided by ETHYDCO.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D792
ESCR 100% Igepal® 3.0 hour
@Temperature 50.0 °C
3.0 hour
@Temperature 122 °F
F50; ASTM D1693
Melt Index of Compound 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5757ASTM D2240, ISO/IEC 17025:1999
Tensile Strength at Break 13.8 MPa2000 psiASTM D638, ISO 527
Tensile Strength, Yield 28.3 MPa4100 psiASTM D638, ISO 527
Elongation at Break 250 %250 %ASTM D638, ISO 527
Elongation at Yield 7.0 %7.0 %ASTM D638, ISO 527
Flexural Modulus 1.15 GPa167 ksiASTM D790B, ISO 178,
Tensile Impact Strength 42.0 kJ/m²20.0 ft-lb/in²Type S; ASTM D1822, ISO 8256
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FASTM D3418, ISO 3146
Crystallization Temperature 117 °C243 °FASTM D3418, ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C163 °FUnannealed; ASTM D648, ISO 75
Vicat Softening Point 127 °C261 °FASTM D1525, ISO 306
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746, ISO 974( E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BorPURE™ MB6561 High Density Polyethylene for Injection Molding
A. Schulman LP481 Molding Grade High-Density Polyethylene
Braskem GE7252 Injection Molding High Density Polyethylene
Braskem HA7260 HDPE Injection Molding Polyethylene
Braskem IA58 HDPE Injection Molding Polyethylene Copolymer

PETHYD917 / 200063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.