MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon® L4434 High Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Applications
ALATHON L 4434 is a medium molecular weight high density copolymer for use in blown film applications. Typical applications include blown film over pouches.

Regulatory Status
L 4434 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing L 4434 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D792
Water Vapor Transmission 2.90 g/m²/day0.187 g/100 in²/dayASTM F1249
Thickness 50.8 microns2.00 milBlown Film; 2.5:1 BUR; 60 mil die gap
Melt Flow 0.34 g/10 min0.34 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 22.1 MPa3200 psiASTM D882
Film Tensile Strength at Yield, TD 27.6 MPa4000 psiASTM D882
Film Elongation at Break, MD 590 %590 %ASTM D882
Film Elongation at Break, TD 850 %850 %ASTM D882
Secant Modulus, MD 0.679 GPa98.5 ksiASTM E111
Secant Modulus, TD 0.910 GPa132 ksiASTM E111
Elmendorf Tear Strength MD 49 g49 gASTM D1922
Elmendorf Tear Strength TD 1100 g1100 gASTM D1922
Elmendorf Tear Strength, MD 0.965 g/micron24.5 g/milASTM D1922
Elmendorf Tear Strength, TD 21.7 g/micron550 g/milASTM D1922
Film Tensile Strength at Break, MD 51.4 MPa7450 psiASTM D882
Film Tensile Strength at Break, TD 46.2 MPa6700 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 127.2 °C<= 261.0 °FDSC; Lyondell Test
Vicat Softening Point 124.3 °C255.7 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 232 °C410 - 450 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding
Braskem F020HC High Crystallinity Polypropylene Homopolymer
Braskem 6D20 Polypropylene Random Copolymer
Chevron Phillips Marlex® 9708 HDPE Injection Molding Resin

PEQU0132 / 36561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.