MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unitika AX-1500 Conditioned
Categories: Polymer; Thermoplastic; Polyarylate

Material Notes: AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in moldability and provide molded products fewer in the number of sink marks, warps, and runoffs.

Characteristics:

  • Nonreinforced heat resistance: Deflection temperature under load without reinforcement: 1.8 MPa at 150°C
  • Chemical resistance: As high as those of polyamide resins, except alkali resistance
  • Adhesiveness: Chemical resistance and adhesiveness as high as those of crystalline resins
  • Lubrication: As high as those of polyamide resins
  • Molding accuracy: Fewer in the number of sink marks and warps, and lower (less than 1/3) in water absorption than polyamide resins

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psiASTM D638
Elongation at Break 70 %70 %ASTM D638
Flexural Strength 76.0 MPa11000 psiASTM D790
Flexural Modulus 1.20 GPa174 ksiASTM D790
Izod Impact, Notched 1.96 J/cm
@Thickness 3.17 mm
3.67 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM D257
Dielectric Constant 3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 25.0 kV/mm635 kV/inASTM D149
Dissipation Factor 0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index >= 600 V>= 600 V
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 230 °C410 - 446 °F
Middle Barrel Temperature 240 - 260 °C464 - 500 °F
Front Barrel Temperature 250 - 270 °C482 - 518 °F
Nozzle Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °Factual surface temp
Drying Temperature 100 °C212 °F
Dry Time 10.0 - 24.0 hour10.0 - 24.0 hour
Back Pressure 0.490 - 1.47 MPa71.1 - 213 psigage pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Ardel® Polyarylate
Unitika C300VN
Unitika U-100 Engineering Plastic
Unitika AXG-1500-300 Conditioned
Unitika U-8400H

PUNITIK892 / 177912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.