MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Zytel® 73G15HSL BK363 PA6-GF15
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: 15% Glass Reinforced, Heat Stabilized, Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³DAM; ISO 1183
Water Absorption 7.6 %
@Thickness 2.00 mm
7.6 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 2.50 %
@Thickness 2.00 mm
2.50 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Number 145 cm³/g1.45 dl/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 123 MPa17800 psiH 961/30; 50% RH; ISO 2039-1
 210 MPa30500 psiH 961/30; DAM; ISO 2039-1
Tensile Strength at Break 80.0 MPa11600 psi50% RH; ISO 527-1/-2
 130 MPa18900 psiDAM; ISO 527-1/-2
Elongation at Break 2.3 %2.3 %DAM; ISO 527-1/-2
 10 %10 %50% RH; ISO 527-1/-2
Tensile Modulus 4.00 GPa580 ksi50% RH; ISO 527-1/-2
 6.50 GPa943 ksiDAM; ISO 527-1/-2
Flexural Strength 90.0 MPa13100 psi50% RH; ISO 178
 190 MPa27600 psiDAM; ISO 178
Flexural Modulus 3.10 GPa450 ksi50% RH; ISO 178
 5.60 GPa812 ksiDAM; ISO 178
Poissons Ratio 0.350.35DAM
 0.360.3650% RH
Izod Impact, Unnotched (ISO)  6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1U
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 21.5 kV/mm546 kV/inDAM; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 16.0 µm/m-°C8.89 µin/in-°FDAM; ISO 11359-1/-2
 15.0 µm/m-°C
@Temperature 55.0 - 160 °C
8.33 µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
 35.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
19.4 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FDAM; ISO 11359-1/-2
 78.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
43.3 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
 100 µm/m-°C
@Temperature 55.0 - 160 °C
55.6 µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
Thermal Conductivity 0.200 W/m-K
@Temperature 270 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 518 °F
Melt
Melting Point 221 °C430 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 204 °C399 °FDAM; ISO 75-1/-2
Vicat Softening Point 215 °C419 °F50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 15.0 °C59.0 °F10°C/min; 50% RH; ISO 11357-1/-2
 55.0 °C131 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread 25.0 mm/min
@Thickness 1.00 mm
0.984 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 21 %21 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °FOptimum, Injection
 260 - 280 °C500 - 536 °FRange, Injection
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FOptimum, Injection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)8.5VDA 277, DS
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0G-value (condensate); ISO 6452; DAM
ISO designationISO 16396-PA6,GF15,M1CGHL1R,S14-060
Max. screw tangential speed (m/s)0.2Injection
Odor Class4VDA 270; DS
Part Marking Code>PA6-GF15<ISO 11469
PolymerPA6-GF15
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA6-GF15ISO 1043
Weather stability delta E1.9DIN 53236
Weather stability grey scale4ISO 105-A02

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 73G15L NC010 PA6-GF15
DuPont Mobility and Materials Zytel® 73G30HSL BK261 PA6-GF30
DuPont Mobility and Materials Zytel® 7301 NC010 PA6
Celanese Zytel® 70G33HS1L NC010 PA66-GF33
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Filled

PDSX5350 / 197990

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.