MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Addiplast Addinyl PMD 20164 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: High resistance to repeated impacts

Information provided by Addiplast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080Conditioned; ISO 868
 8282ISO 868
Tensile Strength at Break 90.0 MPa13100 psiConditioned; ISO R 527
 130 MPa18900 psiISO R 527
Elongation at Yield 4.0 %4.0 %ISO R 527
 6.0 %6.0 %Conditioned; ISO R 527
Modulus of Elasticity 5.00 GPa725 ksiConditioned; ISO 178
 8.00 GPa1160 ksiISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²ISO 180/1A
 25.0 kJ/m²11.9 ft-lb/in²Conditioned; ISO 180/1A
Charpy Impact Unnotched 8.00 J/cm²38.1 ft-lb/in²ISO 179/IeU
 9.00 J/cm²42.8 ft-lb/in²Conditioned; ISO 179/IeU
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179/IeA
 2.50 J/cm²11.9 ft-lb/in²Conditioned; ISO 179/IeA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; CEI 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmCEI 60093
Comparative Tracking Index >= 600 V>= 600 VCEI 60112/Solution A
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75-2/AF

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron™ CMP XL20 PAI
Mitsubishi Chemical Advanced Materials Duratron™ T4203 PAI Extruded Polyamide-imide
Asahi Kasei Leona™ 91G60 Polyamide 66, MF Reinforced
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole

PFADD882 / 156096

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.