MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aldrich Single Layer Graphene on PET
Categories: Carbon; Polymer; Film; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: PET film base with graphene coating; uniform film and excellent thickness consistency. Its transparency combined with electrical conductivity allows it use in many niche applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 188 microns7.40 milPET
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 132 %132 %
Film Elongation at Break, TD 99 %99 %
Coefficient of Friction, Dynamic 0.40.4
Coefficient of Friction, Static 0.460.46
Film Tensile Strength at Break, MD 179 MPa26000 psi
Film Tensile Strength at Break, TD 197 MPa28600 psi
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 500 ohm500 ohmGraphene
 
Optical PropertiesMetricEnglishComments
Haze 0.90 %0.90 %PET
Transmission, Visible 92 %92 %PET
 >= 95 %>= 95 %Graphene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow CVD Graphene Film on PET
XG Sciences xGnP® Graphene Nanoplatelets
Goodfellow CVD Graphene Film on Quartz Glass
SunChemical Gwent P2121112P1 Acid Vapor Plasma Modified Graphene Nanoplatelets
Goodfellow CVD Graphene Film on Copper Foil

PSIGMA990 / 159764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.