MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: HE3490-LS is a black, bimodal, high density polyethylene classified as an MRS 10.0 material (PE100) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an optimized stabilization system.

HE3490-LS is recommended for pressure pipe systems in the applications field of drinking water and natural gas, pressure sewerage, relining, sea outfall and industrial. It is especially designed fro the production of larger diameter, thick wall pipe, but can be processed for the whole range of diameters. It also shows excellent resistance to rapid crack propagation and slow crack growth.

Former trade name for this product was Borstar®.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³Base Resin; ISO 1183/ISO 1872-2B
 0.960 g/cc0.0347 lb/in³Compound; ISO 1183/ISO 1872-2B
ESCR 10% Igepal® >= 10000 hour>= 10000 hourASTM D1693-A
Carbon Black Loading 2.0 %2.0 %ASTM D1603
Melt Flow  >= 0.10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
>= 0.10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 0.25 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ISO 868
Tensile Strength, Yield 24.99 MPa3625 psiAt 50 mm/min; ISO 527-2
Elongation at Break >= 600 %>= 600 %ISO 527-2
Charpy Impact, Notched 1.60 J/cm²
@Temperature 0.000 °C
7.61 ft-lb/in²
@Temperature 32.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Die Temperature 200 - 210 °C392 - 410 °F
Melt Temperature 200 - 220 °C392 - 428 °F
Head Temperature 200 - 210 °C392 - 410 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes
Borealis BorSafe™ HE3470-LS Black HDPE Compound for Pressure Pipes
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes
Borealis Borstar® HE3474-LS Blue HDPE Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Drinking Water

PBOREA121 / 27428

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.