MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

East Coast Precision Manufacturing
East Coast Precision Manufacturing - Vespel® Machining

TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber  (discontinued **)
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automotive applications such as shock absorbers, seals, gaskets, bushings, boots, and hoses.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/cc
Mooney Viscosity 30 - 60
@Temperature 100 °C
30 - 60
@Temperature 212 °F
ML(5+4), preliminary
Permeability 3.2e-83.2e-8Gas, N2; 80ºC, 345kPa; cm²/sec-atm; Formulation Example; Press Cure 7'/177ºC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6262Formulation Example; Press Cure 7'/177ºC
Tensile Strength 27.3 MPa3960 psiFormulation Example; Press Cure 7'/177ºC
 <= 27.6 MPa<= 4000 psi
Elongation at Break 446 %446 %Formulation Example; Press Cure 7'/177ºC
100% Modulus 2.20 MPa
@Strain 100 %
319 psi
@Strain 100 %
Formulation Example; Press Cure 7'/177ºC
200% Modulus 5.30 MPa
@Strain 200 %
769 psi
@Strain 200 %
Formulation Example; Press Cure 7'/177ºC
300% Modulus 13.3 MPa
@Strain 300 %
1930 psi
@Strain 300 %
Formulation Example; Press Cure 7'/177ºC
Resilience 40 - 4540 - 45percent
 4444Bashore Resilience (%)
Tear Strength <= 22.6 kN/m<= 129 pliDie C; Formulation Example; Press Cure 7'/177ºC
 <= 35.0 kN/m<= 200 pli
Compression Set 7.2 %
@Temperature 80.0 °C,
Time 79200 sec
7.2 %
@Temperature 176 °F,
Time 22.0 hour
Formulation Example; Press Cure 7'/177ºC
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 - 20.0 min0.0833 - 0.333 hourfor compression molded lab sheets
Shelf Life 12.0 Month12.0 Monthunder dry and cool conditions
 
Descriptive Properties
Abrasion ResistanceVery good
AppearancePale to light amber solid bale or milled sheets
DIN Abrasion (mm³)77.4Loss; Formulation Example; Press Cure 7'/177ºC
Formulation as Tested0.3Stearic Acid
 0.5TAC
 1Struktol WB222
 1Low Melt Polyethylene
 100Millathane 28
 20N990 Black
 4DBPH 50%
OdorFaint, characteristic
Ozone ResistanceExcellent
Package Weight (lbs)50

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mearthane Durethane™ C 10-30A Polyurethane
ATG s.r.l. AU-EU Polyurethane Rubber
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
TSE Industries Millathane® 66 Millable Polyurethane Rubber
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber

PMILL009 / 87053

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.