MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Sheets
Categories: Polymer; Thermoset; Melamine; Melamine Formaldehyde, Molded, Glass Fiber Filler

Material Notes: Description: Melamine-based composite material reinforced with glass fabric. High arc resistance and tracking resistance. Flame-resistant. Self-extinguishing.

Information provided by Elektro-Isola

Key Words: IEC/EN 60893-3-1 MF GC 201, DIN 7735 Hgw 2272, BS 3953 MF-4, NEMA LI 1 G-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc
@Temperature 23.0 °C
0.0723 lb/in³
@Temperature 73.4 °F
24h/23°C/50% RH; ISO 1183-A
Water Absorption 1.3 %1.3 %ISO 62-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 250 MPa
@Thickness >=1.50 mm
36300 psi
@Thickness >=0.0591 in
24h/23°C/50% RH; ISO 527
Flexural Strength 350 MPa
@Thickness >=1.50 mm,
Temperature 23.0 °C
50800 psi
@Thickness >=0.0591 in,
Temperature 73.4 °F
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Flexural Modulus 18.0 GPa
@Thickness >=1.50 mm
2610 ksi
@Thickness >=0.0591 in
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Compressive Strength 450 MPa
@Thickness >=5.00 mm
65300 psi
@Thickness >=0.197 in
24h/23°C/50% RH, , Normal to laminate plane; ISO 604
Shear Strength 30.0 MPa
@Thickness >=5.00 mm
4350 psi
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; IEC 60893-2
Izod Impact, Notched (ISO) 60.0 kJ/m²
@Thickness >=5.00 mm
28.6 ft-lb/in²
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; ISO 180/2A
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+8 ohm1.00e+8 ohmafter immersion in water for 24 hr at 23°C; IEC 60167
Dielectric Constant 5.5
@Thickness <=3.00 mm,
Frequency 50 Hz
5.5
@Thickness <=0.118 in,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Dielectric Strength  0.787 kV/mm
@Thickness >=3.00 mm,
Temperature 90.0 °C
20.0 kV/in
@Thickness >=0.118 in,
Temperature 194 °F
after 1 hour in oil, Parallel to laminate plane; IEC 60243-1
 5.00 kV/mm
@Thickness 3.00 mm,
Temperature 90.0 °C
127 kV/in
@Thickness 0.118 in,
Temperature 194 °F
after 1 hour in oil, Normal to laminate plane; IEC 60243-1
Dissipation Factor 0.010
@Thickness <=3.00 mm,
Frequency 50 Hz
0.010
@Thickness <=0.118 in,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Comparative Tracking Index 600 V
@Thickness >=3.00 mm
600 V
@Thickness >=0.118 in
24h/23°C/50% RH; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C
@Thickness >=3.00 mm,
Time 7.20e+7 sec
266 °F
@Thickness >=0.118 in,
Time 20000 hour
IEC 60216
Flammability Test 5.0
@Thickness 3.00 mm
5.0
@Thickness 0.118 in
IEC 60695-11-10
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube
Perstorp Compounds AMITEC 751 Melamine
Bakelite® PF 31 Phenolic Formaldehyde Resin, UL Listed
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet
Perstorp Compounds Aminel FX Melamine

PELEKT050 / 126926

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.