MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bohler-Uddeholm M238 VMR® P20 Plastic Lens Mold Steel  (discontinued **)
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: M238 VMR is a vacuum arc remelted, hardened and tempered plastic mold steel with excellent cleanliness for best polishability ideal for lens mold tooling. The hardness is consistent over the entire cross-section of the steel block, even in large sizes, due to the addition of nickel.
  • Minimum gas contents
  • Reduction of trace elements such as Pb, Bi, Te, As, Sn, Sb
  • Minimum microsegregations at the center of ingot
  • Low susceptibility to the formation of freckles (segregation)
  • Highly precise chemical analysis
Applications: Lens mold tooling, mold carrier frames for plastic molds, components for general mechanical engineering and tool manufacture where highest polishability and fatigue strength are required.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5454without tempering
Tensile Strength, Ultimate 2000 MPa290000 psiat HRC 54
Modulus of Elasticity 210 GPa30500 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000190 ohm-cm0.0000190 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.8 µm/m-°C
@Temperature 20.0 - 100 °C
7.11 µin/in-°F
@Temperature 68.0 - 212 °F
 13.0 µm/m-°C
@Temperature 20.0 - 200 °C
7.22 µin/in-°F
@Temperature 68.0 - 392 °F
 13.8 µm/m-°C
@Temperature 20.0 - 300 °C
7.67 µin/in-°F
@Temperature 68.0 - 572 °F
 14.0 µm/m-°C
@Temperature 20.0 - 400 °C
7.78 µin/in-°F
@Temperature 68.0 - 752 °F
 14.2 µm/m-°C
@Temperature 20.0 - 500 °C
7.89 µin/in-°F
@Temperature 68.0 - 932 °F
 14.2 µm/m-°C
@Temperature 20.0 - 600 °C
7.89 µin/in-°F
@Temperature 68.0 - 1110 °F
 14.5 µm/m-°C
@Temperature 20.0 - 700 °C
8.06 µin/in-°F
@Temperature 68.0 - 1290 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity  34.0 W/m-K
@Temperature 20.0 °C
236 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 34.5 W/m-K
@Temperature 100 °C
239 BTU-in/hr-ft²-°F
@Temperature 212 °F
 34.5 W/m-K
@Temperature 200 °C
239 BTU-in/hr-ft²-°F
@Temperature 392 °F
 35.0 W/m-K
@Temperature 300 °C
243 BTU-in/hr-ft²-°F
@Temperature 572 °F
 35.0 W/m-K
@Temperature 400 °C
243 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 %0.38 %
Chromium, Cr 2.0 %2.0 %
Iron, Fe 94.52 %94.52 %As Balance
Manganese, Mn 1.5 %1.5 %
Molybdenum, Mo 0.20 %0.20 %
Nickel, Ni 1.1 %1.1 %
Silicon, Si 0.30 %0.30 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM RAMAX® LH Plastic Mold Steel
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
AISI Type P20 Mold Steel (UNS T51620)
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel
Bohler-Uddeholm IMPAX® P20 Hot Work Tool Steel

NBUCOR41 / 98120

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.