MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestamid® E62-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Nylon (Polyamide PA); Nylon 12 (PA12); Polyether Block Amide (PEBA)

Material Notes: Description: Compared to other contending thermoplastic elastomers, PA 12 elastomers are distinguished by the following properties:
  • They have low density.
  • They are highly resistant to chemicals and solvents.
  • They are easy to process and color and are easy to overmold.
  • They can be decorated easily by means of heat transfer printing.
  • They have excellent impact strength at low temperatures.
  • Their hardness and flexibility can be varied over a wide range.
  • They have high elasticity and good recovery.
  • Their mechanical properties are only slightly temperature-dependent.
  • They are free of volatile or migrating plasticizers.

Applications: alpine ski boots, noiseless gears, conveyor belts

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Water Absorption at Saturation 1.1 %1.1 %ISO 62
Viscosity Number 190 cm³/g1.90 dl/gISO 307
Linear Mold Shrinkage 0.0060 - 0.011 cm/cm
@Thickness 3.00 mm
0.0060 - 0.011 in/in
@Thickness 0.118 in
sheet with film gate at rim, mold temperature 80°C
Linear Mold Shrinkage, Transverse 0.0090 - 0.014 cm/cm
@Thickness 3.00 mm
0.0090 - 0.014 in/in
@Thickness 0.118 in
sheet with film gate at rim, mold temperature 80°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ISO 868
Tensile Strength at Break 42.0 MPa6090 psiISO 527-1, ISO 527-2
Elongation at Break >= 200 %>= 200 %ISO 527-1, ISO 527-2
Tensile Modulus 0.370 GPa53.7 ksiISO 527-1, ISO 527-2
50% Modulus 23.0 MPa
@Strain 50 %
23.0 MPa
@Strain 50 %
ISO 527-1, ISO 527-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
Partial Break; ISO 179/1eA
Tensile Creep Modulus, 1000 hours 200 MPa29000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmSpec.; IEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmSpec.; IEC 60093
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
 9.0
@Frequency 100 Hz
9.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 39.0 kV/mm991 kV/inK20/P50; IEC 60243-1
Dissipation Factor  0.10
@Frequency 100 Hz
0.10
@Frequency 100 Hz
IEC 60250
 0.12
@Frequency 1e+6 Hz
0.12
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 55.0 °C
111 µin/in-°F
@Temperature 73.4 - 131 °F
Longitudinal; ISO 11359
CTE, linear, Transverse to Flow 200 µm/m-°C
@Temperature 23.0 - 55.0 °C
111 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1
Vicat Softening Point 110 °C230 °F50N; ISO 306
 165 °C329 °F10N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestamid® EX9200 Heat & Light Stabilized Nylon 12/PEBA Elastomer
Evonik Vestamid® E40-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer
Evonik Vestamid® E62-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer for Fiber Optic Jacketing
Evonik Vestamid® L2140 Nylon 12
Arkema Pebax® 7433 SA 01 MED TPA

PHULA21 / 47381

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.