MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Elvax® 150W-LG Ethylene Vinyl Acetate  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: DuPont™ Elvax® 150W-LG is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the pellets from blocking, low levels of a (W) amide additive is added to the polymer. Additive: antiblock

Applications:Elvax® 150W-LG resins can be used for the following applications: adhesives, sealants, and wax blends; wire and cable applications.

Information provided by DuPont™

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³ASTM D792-ISO 1183
Vinyl Acetate Content 32 %32 %
Melt Flow 43 g/10 min
@Load 2.16 kg,
Temperature 190 °C
43 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565ASTM D2240-ISO 868
 
Thermal PropertiesMetricEnglishComments
Melting Point 63.0 °C145 °FASTM D3417
Vicat Softening Point 36.0 °C96.8 °FASTM D1525, ISO 306
Ring & Ball Softening Point 110 °C230 °FASTM E28
 
Descriptive Properties
Cloud Point in Paraffin Wax, °C10210% Elvax® in fully refined paraffin wax, 146 AMP. Incompatible at temperatures up to 177°C.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvax® 150W Ethylene Vinyl Acetate
Dow Elvax® 3190A Ethylene Vinyl Acetate
DuPont Elvax® 210 Ethylene Vinyl Acetate
DuPont Elvax® 205W Ethylene Vinyl Acetate
DuPont Elvax® 3121A Ethylene-Vinyl Acetate Copolymer Resin for Blown Film

PDUP930 / 33497

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.