MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® 2710IR PA66, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: TECHNYL® 2710 IR is an unfilled polyamide 6.6, impact modified, for injection molding. The product is available in natural color, and in colors on request.

Benefits: This product, used in all sector of industry, offers an excellent productivity due to a fast cycle time. It has also a very good surface aspect after molding.

Key Properties: Medium impact, Good surface aspect, and Fast cycle

Available in: Asia Pacific

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC.This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications

Applications: Battery gaskets, fasteners.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
1.1 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.019 cm/cm0.019 in/in
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 65.0 MPa9430 psiISO 527 type 1 A
Elongation at Break 25 %25 %ISO 527 Type 1A
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 2.10 GPa305 ksiISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²10.5 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 3.23.2IEC60250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 475 V475 VSolution B; IEC 60112
 550 V550 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 185 °F
Melting Point 262 °C504 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C198 °FISO 75/Af
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
ISO 1210
Oxygen Index 21 %21 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Feed Temperature 265 - 270 °C509 - 518 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® 2710IR PA66, Conditioned
Domo TECHNYL® A 221 Natural FA PA66, DRY
Domo TECHNYL® 27010ST PA66, DRY
Domo TECHNYL® A 205F PA66, DRY
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0

PRHOD578 / 137809

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.