MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyetherketoneketone (PEKK), Unreinforced
Categories: Polymer; Thermoplastic; Polyketone; PEKK, Unreinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.27 - 1.31 g/cc0.0459 - 0.0473 lb/in³Average value: 1.28 g/cc Grade Count:20
Water Absorption 0.100 - 0.600 %0.100 - 0.600 %Average value: 0.260 % Grade Count:5
Moisture Absorption at Equilibrium 0.150 - 0.600 %0.150 - 0.600 %Average value: 0.300 % Grade Count:3
Linear Mold Shrinkage 0.00500 - 0.0160 cm/cm0.00500 - 0.0160 in/inAverage value: 0.00950 cm/cm Grade Count:4
Melt Flow 6.00 - 120 g/10 min6.00 - 120 g/10 minAverage value: 30.3 g/10 min Grade Count:12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 86.0 - 88.086.0 - 88.0Average value: 87.3 Grade Count:3
Tensile Strength, Ultimate 40.6 - 111 MPa5890 - 16100 psiAverage value: 76.2 MPa Grade Count:13
 25.9 - 116.5 MPa
@Temperature -184 - 149 °C
3760 - 16900 psi
@Temperature -300 - 300 °F
Average value: 68.0 MPa Grade Count:1
Tensile Strength, Yield 40.6 - 95.0 MPa5890 - 13800 psiAverage value: 78.7 MPa Grade Count:5
Elongation at Break 0.940 - 80.0 %0.940 - 80.0 %Average value: 13.4 % Grade Count:13
 1.20 - 23.5 %
@Temperature -184 - 149 °C
1.20 - 23.5 %
@Temperature -300 - 300 °F
Average value: 5.76 % Grade Count:1
Elongation at Yield 0.580 - 4.89 %0.580 - 4.89 %Average value: 3.61 % Grade Count:5
Modulus of Elasticity 2.68 - 6.56 GPa389 - 952 ksiAverage value: 3.61 GPa Grade Count:20
 1.441 - 8.074 GPa
@Temperature -184 - 149 °C
209.0 - 1171 ksi
@Temperature -300 - 300 °F
Average value: 5.03 GPa Grade Count:1
Flexural Yield Strength 54.0 - 193 MPa7830 - 28000 psiAverage value: 124 MPa Grade Count:12
Flexural Modulus 2.50 - 5.54 GPa363 - 804 ksiAverage value: 3.37 GPa Grade Count:12
Flexural Strain at Break 1.40 - 6.00 %1.40 - 6.00 %Average value: 3.26 % Grade Count:7
Compressive Yield Strength 90.6 - 207 MPa13100 - 30000 psiAverage value: 117 MPa Grade Count:9
Compressive Modulus 2.12 - 5.86 GPa307 - 850 ksiAverage value: 2.86 GPa Grade Count:6
Poissons Ratio 0.330 - 0.4500.330 - 0.450Average value: 0.390 Grade Count:4
Shear Modulus 1.17 - 1.57 GPa170 - 228 ksiAverage value: 1.44 GPa Grade Count:3
Izod Impact, Notched 0.220 - 0.630 J/cm0.412 - 1.18 ft-lb/inAverage value: 0.399 J/cm Grade Count:8
Izod Impact, Unnotched 0.470 - 30.8 J/cm0.881 - 57.7 ft-lb/inAverage value: 8.66 J/cm Grade Count:5
Charpy Impact Unnotched 2.20 J/cm² - NB10.5 ft-lb/in² - NBAverage value: 4.87 J/cm² Grade Count:8
 1.80 J/cm² - NB
@Temperature -30.0 - -30.0 °C
8.57 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 3.72 J/cm² Grade Count:7
Charpy Impact, Notched 0.450 - 0.550 J/cm²2.14 - 2.62 ft-lb/in²Average value: 0.488 J/cm² Grade Count:8
 0.400 - 0.500 J/cm²
@Temperature -30.0 - -30.0 °C
1.90 - 2.38 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.457 J/cm² Grade Count:7
Coefficient of Friction 0.173 - 0.1860.173 - 0.186Average value: 0.177 Grade Count:3
Coefficient of Friction, Static 0.262 - 0.2850.262 - 0.285Average value: 0.270 Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3820 - 1.00e+16 ohm-cm3820 - 1.00e+16 ohm-cmAverage value: 2.73e+15 ohm-cm Grade Count:10
Surface Resistance 8.43 - 2.00e+16 ohm8.43 - 2.00e+16 ohmAverage value: 8.57e+15 ohm Grade Count:6
Dielectric Constant 2.50 - 3.322.50 - 3.32Average value: 2.95 Grade Count:13
Dielectric Strength 23.6 - 84.0 kV/mm599 - 2130 kV/inAverage value: 47.8 kV/mm Grade Count:4
Dissipation Factor 0.00300 - 0.004000.00300 - 0.00400Average value: 0.00363 Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.0 - 77.0 µm/m-°C11.7 - 42.8 µin/in-°FAverage value: 42.8 µm/m-°C Grade Count:5
 34.74 - 59.22 µm/m-°C
@Temperature 30.0 - 150 °C
19.30 - 32.90 µin/in-°F
@Temperature 86.0 - 302 °F
Average value: 46.5 µm/m-°C Grade Count:4
Thermal Conductivity 0.250 - 0.470 W/m-K1.74 - 3.26 BTU-in/hr-ft²-°FAverage value: 0.329 W/m-K Grade Count:4
Melting Point 300 - 360 °C572 - 680 °FAverage value: 318 °C Grade Count:7
Maximum Service Temperature, Air 149 - 300 °C300 - 572 °FAverage value: 228 °C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 150 - 277 °C302 - 531 °FAverage value: 170 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 139 - 185 °C282 - 365 °FAverage value: 157 °C Grade Count:18
Glass Transition Temp, Tg 149 - 160 °C300 - 320 °FAverage value: 156 °C Grade Count:11
Flammability, UL94 V-0V-0Grade Count:5
Smoke Density 10.010.0Average value: 10.0 Grade Count:3
Oxygen Index 35.0 - 40.0 %35.0 - 40.0 %Average value: 37.5 % Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyetherimide (PEI)
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Acrylic, Extruded

O2169 / 77942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.