MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daicel CEVIAN® B1500 PBT/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/Polyester Alloy; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Unfilled, Excellent Toughness

These are typical values and are not intended for specification purposes. UL approved file No. is E47773.

Information provided by PlastxWorld Inc.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/inASTM D955
Melt Flow 15 g/10 min15 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104104ASTM D785
Tensile Strength, Yield 42.1 MPa6100 psiASTM 638
Elongation at Break 100 %100 %ASTM D638
Flexural Yield Strength 62.7 MPa9100 psiASTM D790
Flexural Modulus 1.93 GPa280 ksiASTM D790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.17 mm
1.30 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °F0.25 inch; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °F0.25 inch; ASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daicel CEVIAN® B1700 PBT/ABS Alloy
Daicel CEVIAN® B14E0 PBT/ABS Alloy
Americhem Engineered Compounds ColorFast® PCT2014 PC/PBT Alloy
E-Polymers Tekaloy® T80 , Dimensional Stability PBT/ABS Alloy
Daicel CEVIAN® B45M0 PBT/ABS Alloy

PPLASTX16 / 56420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.